Processing Gold Ore by Flotation
For example, where flotation took place immediately after vanning, the residue assayed $2.60 gold and 0.30% copper, but where tailing from panning was allowed to remain under water for 6 hours before flotation, the residue assayed $3.10 gold and 0.67% copper.