Epoxy resins composites for X-ray shielding materials additivated …
Eq. (1) gives, using A = 1 :3 m 2 /g a range from 3 × 10 −3 g of surfactant per gram of barite to 1.6 × 10 −2 g of surfactant per gram of barite as showed in Fig. 4.Functionalized barites were prepared in LAG conditions [22], [23] using SA or SDS. The functionalized barites (together with bare barites as references) were used to prepare additive/epoxy resin …